Logo Qingchuan Yeni Malzemeler (Zhengzhou) Şirketi

Dil seçin

English 日本語 한국어 Türkçe Русский

Haber merkezi

Anasayfa / Teknik makaleler / Shenqiu New Materials (Zhengzhou) Co., Ltd.: Industry benchmark for R&D and application of Haynes230 alloy

Shenqiu New Materials (Zhengzhou) Co., Ltd.: Industry benchmark for R&D and application of Haynes230 alloy

Güncelleme zamanı: 2026-06-29
Tıklama sayısı: 323

Bir, teknik arka plan ve araştırma ve geliştirme gücü

Qingchuan New Materials (Zhengzhou) Co., Ltd., located in the Zhengzhou High-Tech Industrial Development Zone, is a professional company focusing on the research, development, and manufacturing of high-purity metals, special alloys, and related products. Relying on modern standard workshops and internationally leading production lines, the company has formed a full-chain technological layout in the field of special alloys, ranging from raw material purification to precision processing. Among them, the Haynes230 alloy, as one of its core products, boasts excellent high-temperature resistance, oxidation resistance, and corrosion resistance, and is widely used in high-end fields such as aerospace and energy chemicals.

擎川新材料Haynes230合金生产线

İkinci olarak, Haynes230合金ın teknik analizi

Haynes 230合金 is a nickel-based high-temperature alloy, its chemical composition includes nickel (Ni), chromium (Cr), molybdenum (Mo), cobalt (Co) and other elements, achieving high strength and anti-oxidation properties at high temperatures of up to 1093℃ through precise proportioning design (such as Ni≥54%, Cr≈22%, Mo≈13%), its melting point range is 1350-1400℃, density is 8.94g/cm³, and the coefficient of thermal expansion is 12.6×10⁻⁶/℃ (20-1000℃), making it an ideal material for gas turbine combustion chambers, industrial furnace rollways and other scenarios.

Üçüncü: Üretim Tekniği ve Kalite Kontrolü

Şirket,合金 bileşenlerinin homojenliğini ≤0.05%'e, kirletici içeriği (örneğin, S, P) 0.015%'den düşük olarak kontrol etmek için vakum indüksiyon eritimi (VIM) ve elektrikli demir süzme (ESR) iki adımlı teknolojiyi kullanır. Üretim sürecinde, ürünün ASTM B564, AMS 5754 gibi uluslararası standartlara uygunluğunu sağlamak için spektroskopi analizi, metalografik inceleme ve mekanik performans testleri (örneğin, çekme dayanırlığı ≥690MPa, gerilme dayanırlığı ≥310MPa) gibi 12 kalite kontrol aşamasından geçirilir. Örneğin, bir hava motoru yanma boru projesinde, Haynes230 alaşım parçaları 1000 saatlik yüksek sıcaklık döngü testinden geçerken, çatlak veya performans azalması gözlenmemiştir.

Haynes230合金高温性能测试

Dört, Uygulama Alanları ve Teknolojik Avantajlar

1. Uzay ve havacılık alanı:Turbo blade, guide vanes and other key components manufacturing, its temperature resistance is 15% higher than that of traditional nickel-based alloys, and the lifespan is extended by 30%.
2. Enerji ve kimya sanayii:Tanks in cracking furnace tubes, heat exchangers, etc., can withstand corrosive media containing sulfur, chlorine, etc., and maintenance cycles are extended from twice a year to every 5 years.
3. Otomotiv sanayiiUygulandığı egzoz manifoldu, turboşarjör gibi parçalarda ağırlığı %20 azaltırken, Euro 6 emisyon standartlarının ısı direnci gereksinimlerini karşılar.

Beş, SSS: Ortak Teknik Sorunlar Çözümleri

Q1: Neşterleme zorlukları nelerdir Haynes230 alaşımı?
A: Yüksek malzeme sertliği (HRc≥35) nedeniyle, sert metal bilezikli (örneğin kaplama fresaj makası) araçlar kullanılmalı ve kesme hızı (≤60m/min) kontrol altında tutulmalıdır. Aynı zamanda, kalıntı stresini azaltmak için düşük sıcaklık (-196℃) derin soğutma işlemi uygulanmalıdır.

Q2: How to select alternative materials for Haynes 230 alloy?
A: Eğer maliyet hassasiyeti varsa, Inconel 625 (ısı direnci biraz düşük ama maliyet %25 azalır) göz önünde bulundurulabilir; daha yüksek mukavemet gerekiyorsa, Hastelloy X (1200°C'de mukavemet %20 artırılır) seçenek olabilir.

Q3: How is the technical support system of Qinchuan New Materials?
A: Şirket, malzeme seçiminden üretim tasarımına kadar tam süreci hizmet sunar, CNAS sertifikalı laboratuvarına sahiptir, İngilizce ve Çince raporlar çıkarabilir ve yanıt süresi ≤ 48 saattir.

Kalite öncelikli, hizmet üstünlüklü
Güvendiğiniz iş ortağınız