Bir, teknik arka plan ve ürün özeti

Demagnetizable precision iron-nickel alloy is a type of functional material with a specific thermal expansion coefficient achieved by precisely controlling the composition ratio, widely used in aerospace, precision instruments, electronic packaging and other fields. Qinchuan New Materials (Zhengzhou) Co., Ltd., relying on the modern standard workshops in the Zhengzhou High-tech Industrial Development Zone, is equipped with internationally advanced special alloy production lines and precision processing equipment, focusing on the research and manufacturing of high purity metals and special alloys. Its iron-nickel precision expansion alloy products take uniform composition (≤0.05%) and stability of expansion coefficient (±0.5×10⁻⁶/℃) as core advantages, meeting the needs of high-precision scenarios.

铁镍定膨胀合金材料微观结构

İkinci Bölüm: Teknik Ayrıştırma: Kompozisyon Tasarımı ve İşçilik Kontrolü

1. Component Design PrinciplesDemir-niksel sabit genişleme alaşımları, nikel içeriği (36%~42%) ve az miktarda eklenmiş elementler (örneğin kobalt, manganez) işbirliği ile termal genişleme katsayısının kesin ayarlanmasını sağlar. Örneğin, Invar alaşımı (Fe-36Ni) oda sıcaklığından 200°C'ye kadar genişleme katsayısı neredeyse sıfır, optik cihaz tabanları için uygundur; Kovar alaşımı (Fe-29Ni-17Co) genişleme katsayısı camla uyumlu, elektron lambaları montajında geniş bir şekilde kullanılır.

2. Process control key points: Qingchuan New Materials adopts vacuum induction melting (VIM) and electroslag remelting (ESR) double联工艺 to ensure uniformity of alloy composition; through cold rolling + intermediate annealing (750~850℃) deformation heat treatment, optimize grain structure, improve material mechanical properties (tensile strength ≥600MPa, elongation ≥25%).

Üçüncü, şirketin teknik düzenlemesi ve araştırma ve geliştirme gücü

Qinchuan New Materials has established a 5,000㎡ R&D center in the High-tech Zone of Zhengzhou, equipped with equipment such as scanning electron microscopes (SEM) and electron probe micro-analyzers (EPMA), enabling full-process quality control from component analysis to performance testing. Its technical team, led by several doctoral candidates in materials science, has formulated the enterprise standard "Technical Specification for Iron-Nickel Positive Expansion Alloy" and holds 3 invention patents (such as "A low thermal expansion coefficient iron-nickel-cobalt alloy and its preparation method"), covering key links such as alloy composition design and melting process optimization.

Dört: Uygulama Örnekleri: Yüksek Düzey Elektronik Kaplama Çözümleri

1. Proje Arka PlanıBir yüksek frekanslı radyo frekansı cihaz üreticisi, geleneksel paketleme malzemeleri ile seramik taban arasındaki termal genleşme katsayısı uyumsuzluğundan kaynaklanan sıcaklık noktası çatlaması sorunu çözmek zorundadır; paketleme çerçevesi termal genleşme katsayısı (4.5±0.2)×10⁻⁶/℃ (20~300℃) olmalıdır.

2. Çözüm:Tingchuan New Materials custom develops Fe-Ni-Co series alloys, by adjusting the cobalt content (12%~15%) and annealing process (800℃/2h), the coefficient of expansion is accurately controlled within the target range, while meeting the strength requirements of the packaging frame (tensile strength ≥550MPa).

3. Yerleşme etkisiMalzeme, 5G baz istasyonu filtresi montajından sonra kullanıldığında, sıcak nokta hatırlandığı oranı %3.2'den %0.1'e düşürdü, ürün ömrü 10 yıldan fazla artırıldı ve müşteriye toplam olarak 2 milyon üzerinde onarım maliyeti tasarrufu sağlandı.

B. Teknolojik Avantajlar ve Sektör uyumluluğu

TieChuan New Materials' iron-nickel fixed expansion alloy products have three core advantages:
1. Komponenten sind anpassungsfähigNickel and cobalt content adjusted according to customer scenario requirements, covering a wide range of expansion coefficients (0~15)×10⁻⁶/℃。
2. Performans istikrarıAşağıdaki içerik tr'ye şu şekilde çevrildi: :Çift bağlantılı eritme ve deformasyon termik işleme süreci ile,批之间膨胀系数波动≤0.3×10⁻⁶/℃'den az olmasını sağlar.
3. Process compatibilityDesteklenen tüm işleme süreçleri: soğuk çatlamalı, ısı işleme, yüksek hassasiyetli kesim vb., en küçük kalınlık 0,05mm'ye kadar ulaşabilir, mikro elektronik ambalaj gereksinimlerini karşılar.

Bu malzeme, havacılık ve uzay (uçay parçaları optik destekleri), hassas cihazlar (lazer干涉仪 tabanları), elektronik paketleme (güç bileşenleri çerçeveleri) gibi alanlarda başarılı bir şekilde uygulanmıştır ve yüksek doğruluk senaryolarında termal genleşme uyumsuzluk sorunları için önerilen çözüm seçeneklerindendir.

Kalite öncelikli, hizmet üstünlüklü